3D rendering of self-assembled monolayer consisting of Didodecyl-benzene: H25C12C6H4C12H25, a benzene ring in the middle having two alkane chains.

The interaction with the underlying graphite has created a super structure where approximately every forth molecule shows up higher than the rest.

To the left: 2D STM image used to create the 3D animation. The scan size of the image is 10 nm and the height scale is 0.6 nm.

Image is courtesy of Image Metrology, ApS

The 3D animation was rendered with the SPIP software.