N-Hydroxysuccinimide-activated hexa(ethylene glycol) undecane Thiol (NHS)

Part #: CMT004
Monothiol with N-hydroxysuccinimide functional group. Qty: 10 mg More details...
Price: $84.35
Tell a friend
N-Hydroxysuccinimide-activated hexa(ethylene glycol) undecane Thiol (NHS)
N-Hydroxysuccinimide-activated hexa(ethylene glycol) undecane Thiol (NHS)
Previous Item   Next Item
 
Product Details
Monothiol with N-hydroxysuccinimide functional group
Whitesides monothiol with N-hydroxysuccinimide functional group.

Specifications
Chemical Formula HS - (CH2)11 - (OCH2CH2)6 - OCH2-CO-NHS
Functional Group NHS (N-hydroxysuccinimide)
Formula Weight (FW) 623.8 C29H53NO11S
CAS Number 884597-24-4
Quantity 10mg
Packaging 0.5ml amber-colored, screw-top glass vial
purged with Argon gas
Storage Requirements Store at -20°C in a sealed plastic bag
 
UPS logoSpecial Shipping Requirements
This item is packaged in dry ice to keep it cold during transport. When ordering online, please select the UPS Next Day Air shipping option. For destinations outside of the United States, please select one of the UPS Express options. Orders can ship Monday thru Thursday to locations within the US, and Monday thru Wednesday to non-US addresses.
 
NHS-esters react with primary amines (N-termini of proteins) under physiological conditions to form a covalent amide bond releasing N-hydroxysuccinimide. Typical NHS-ester reactions are performed between pH 7-9 at 4 deg C to room temperature from 30 minutes to 2 hours.
We currently offer Whitesides monothiols and aromatic-dithiols in 10mg quantities. Larger quantities are available upon request.   View all thiol chemicals.
 
Download
Catalog:
Thiol Chemicals Product FlyerPEG-Thiols for Gold Surface Modifications
(170 KB PDF)

Nano Manipulation and Sensing Devices
Nano Manipulation
and Sensing Devices


Science at the Nanoscale: An Introductory Textbook
Nanoscience and
Nanotechnology Books




US & Canada
888-777-5573

(toll free)

International
+1 480-940-3940


The best prices and the largest selection of AFM probes


We have a large number of probes & accessories that are suited for a wide variety of research. Deciding which is best can be difficult. Call us to discuss your application. Each of our technical sales staff has over a decade of experience in AFM.

Nanoscience Rewards Program

We accept: