Aspire CT170

As low as $250.00
In stock
SKU
CT170 -(select options)

Conical Tapping Mode AFM Probe

Ordering Information

Quantity

Coating

Part Number

Price
10
probes
None CT170-10
$250.00*
Al reflex CT170R-10
25
probes
None CT170-25
$550.00*
Al reflex CT170R-25
50
probes
None CT170-50
$990.00*
Al reflex CT170R-50
75
probes
None CT170-75
$1,380.00*
Al reflex CT170R-75
100
probes
None CT170-100
$1,720.00*
Al reflex CT170R-100

*A 10% discount is offered to academic and government institutions. To receive the discount, enter academic10 as the Discount Code during checkout. This discount may not be combined with most other sales, promotions, discounts, codes, coupons and/or offers.


Aspire - Experience the Conical Advantage

The geometry of an AFM tip plays an important role when imaging surfaces. The use of a uniform, conical tip guarantees that you’re acquiring truly symmetrical images. A conical shape is especially beneficial when imaging membranes (holes) and pillar structures, or random structures with surface roughness. Aspire™ AFM probes are the first conically-shaped AFM tips for the mass-market. Manufactured from high-quality, highly doped, single crystal silicon, these probes are robust and offer long imaging life. 

Aspire probe model CT170 is designed for general tapping mode applications and features a typical tip radius of 8 nm. An industry-standard chip design guarantees compatibility with all standard AFM chip holders and also the pre-aligned holders on Nanosurf AFMs*. Model CT170R probes have an aluminum Reflex coating* on the cantilever's detector side. The coating improves laser reflection and does not coat the cantilever's tip.

2 Please contact us about packaging options for half wafers (200 probes) and full wafers (400 probes).
 
Technical Data Typical Value Range
Force Constant 50 N/m 28 - 75 N/m
Resonance Frequency 170 kHz 150 - 210 kHz
Length 225 µm 215 - 235 µm
Width 42 µm 40 - 45 µm
Thickness 6.5 µm 5.5 - 7.5 µm
Shape / Cross-section Rectangular / Rectangular
Number of Cantilevers 1 per chip
Tip Offset ~ 10 µm
Tip Style Conical
Tip Aspect Ratio 1.5:1
Tip Cone Angle 30 degrees
Tip Height 15 µm 12.5 - 17.5 µm
Tip Radius ~ 8 nm < 10 nm
Material Single Crystal Silicon, n-type, highly doped
Chip Size
(industry standard)
3400 µm (L) x 1600 µm (W) x 315 µm (T)
Alignment Grooves Yes
Coating (optional)* Aluminum reflex (on non-tip side)
More Information
Spring Constant (Nominal) 50 N/m
Spring Constant $50.00
Frequency (Nominal) 170 kHz
Frequency $170.00