Nanosensors PPP-XYNCHR

As low as $320.00
In stock
SKU
PPP-XYNCHR -(select options)

Tapping Mode AFM Probe with Special Alignment System

Ordering Information

Quantity

Coating

Part Number

Price
10 
probes
Al Reflex PPP-XYNCHR-10
$320.00
20 
probes
Al Reflex PPP-XYNCHR-20
$573.00
50 
probes
Al Reflex PPP-XYNCHR-50
$1,265.00

The XY-auto-alignment probes for Non-Contact / Tapping mode application (High resonance frequency) with a Reflex coating extend the plug-and-fit alignment concept of the Alignment Chip (ALIGN) to 125 µm short cantilevers optimized for high speed non-contact / tapping mode applications. Probe exchange with a tip repositioning accuracy of better than ± 8 µm is possible for all probes of the XY-alignment probes series - independent of their cantilever length. This series is adjusted to the tip position of probes with a cantilever length of 225 µm.

As a matter of course, the features of the proven Point Probe® Plus series such as high application versatility, compatibility with most commercial SPMs, extremely low and reproducible tip radius as well as a precisely defined tip shape are maintained. The typical tip radius of less than 7 nm and the minimized variation in tip shape provide more reproducible images and enhanced resolution.

NANOSENSORS™ PPP-NCHR AFM probes are designed for non-contact mode or tapping mode AFM (also known as: attractive or dynamic mode). This type of AFM probe combines high operation stability with outstanding sensitivity and fast scanning ability.

The probe offers unique features:

  • guaranteed tip radius of curvature < 10 nm
  • tip height 10 - 15 µm
  • highly doped silicon to dissipate static charge
  • Al coating on detector side of cantilever
  • chemically inert
  • high mechanical Q-factor for high sensitivity
  • tip repositioning accuracy of better than ± 8 µm (in combination with Alignment Chip)

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 4 3.0 - 5.0
Mean Width /µm 30 22.5 - 37.5
Length /µm 125 115 - 135
Force Constant /(N/m) 42 10 - 130
Resonance Frequency /kHz 330 204 - 497
More Information
Spring Constant (Nominal) 42 N/m
Spring Constant $42.00
Frequency (Nominal) 330 kHz
Frequency $330.00
Allow Set Quantities Yes
Featured Yes
Specs

Tapping Mode AFM Probe with Special Alignment System

© 2018 Nanoscience Instruments