NANOSENSORS™ PtSi-NCH probes are designed for non-contact mode or tapping mode AFM (also known as: attractive or dynamic mode). This probe type combines high operation stability with outstanding sensitivity and fast scanning ability.

For applications that require a wear resistant and an electrically conductive tip we recommend this type. NANOSENSORS PtSi-FM probes are suitable for C-AFM, Tunneling AFM and Scanning Capacitance Microscopy (SCM).

The Platinum Silicide coating shows an excellent conductivity (almost approaching metal conductivity). The typical tip radius of curvature is around 25 nm.

The probe offers unique features:

  • platinum silicide coating with excellent conductivity and good wear-out behavior
  • high mechanical Q-factor for high sensitivity
  • alignment grooves on backside of silicon holder chip

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 4 3.0 - 5.0
Mean Width /µm 30 22.5 - 37.5
Length /µm 125 115 - 135
Force Constant /(N/m) 42 10 - 130
Resonance Frequency /kHz 330 204 - 497




More Information
Spring Constant (Nominal) 42 N/m
Spring Constant $42.00
Frequency (Nominal) 330 kHz