NANOSENSORS™ TL-CONT sensors are designed for special applications where no tip at the cantilever is needed.

The probe offers unique features:

  • no tip
  • highly doped silicon to dissipate static charge
  • chemically inert
  • high mechanical Q-factor for high sensitivity

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 2 1.0 - 3.0
Mean Width /µm 50 42.5 - 57.5
Length /µm 450 440 - 460
Force Constant /(N/m) 0.2 0.02 - 0.77
Resonance Frequency /kHz 13 6 - 21
More Information
Spring Constant (Nominal) 0.2 N/m
Spring Constant $0.20
Frequency (Nominal) 13 kHz