Nanosensors TL-FM

As low as $320.00
In stock
SKU
TL-FM -(select options)

Tipless Force Modulation AFM Cantilever

Ordering Information

Quantity

Coating

Part Number

Price
10 
probes
None TL-FM-10
$320.00
20 
probes
None TL-FM-20
$573.00
50 
probes
None TL-FM-50
$1,265.00

NANOSENSORS™ TL-FM probes are designed for special applications where no tip at the cantilever is needed.

The probe offers unique features:

  • no tip
  • highly doped silicon to dissipate static charge
  • chemically inert
  • high mechanical Q-factor for high sensitivity
  • alignment grooves on backside of silicon holder chip
  • precise alignment of the cantilever position (within +/- 2 µm) when used with the Alignment Chip
  • compatible with PointProbe® Plus XY-Alignment Series

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 3 2.0 - 4.0
Mean Width /µm 28 20 - 35
Length /µm 225 215 - 235
Force Constant /(N/m) 2.8 0.5 - 9.5
Resonance Frequency /kHz 75 45 - 115

More Information
Spring Constant (Nominal) 2.8 N/m
Spring Constant $2.80
Frequency (Nominal) 75 kHz
Frequency $75.00
Allow Set Quantities Yes
Featured Yes
Specs

Tipless Force Modulation AFM Cantilever

© 2018 Nanoscience Instruments