NANOSENSORS™ TL-NCH cantilevers are designed for special applications where no tip at the cantilever is needed.

The probe offers unique features:

  • no tip
  • highly doped silicon to dissipate static charge
  • chemically inert
  • high mechanical Q-factor for high sensitivity

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 4 3.0 - 5.0
Mean Width /µm 30 22.5 - 37.5
Length /µm 125 115 - 135
Force Constant /(N/m) 42 10 - 130
Resonance Frequency /kHz 330 204 - 497




More Information
Spring Constant (Nominal) 42 N/m
Spring Constant $42.00
Frequency (Nominal) 330 kHz
Frequency $330.00