Nanosensors TL-NCL

As low as $320.00
In stock
SKU
TL-NCL -(select options)

Tipless, Long Tapping Mode AFM Cantilever

Ordering Information

Quantity

Coating

Part Number

Price
10 
probes
None TL-NCL-10
$320.00
20 
probes
None TL-NCL-20
$573.00
50 
probes
None TL-NCL-50
$1,265.00

NANOSENSORS™ TL-NCL tipless cantilevers are designed for special applications where no tip at the cantilever is needed.

The probe offers unique features:

  • no tip
  • highly doped silicon to dissipate static charge
  • chemically inert
  • high mechanical Q-factor for high sensitivity
  • alignment grooves on backside of silicon holder chip
  • precise alignment of the cantilever position (within +/- 2 µm) in conjunction with the usage of the alignment chip
  • compatible with PointProbe® Plus XY-Alignment Series

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 7 6.0 - 8.0
Mean Width /µm 38 30 - 45
Length /µm 225 215 - 235
Force Constant /(N/m) 48 21 - 98
Resonance Frequency /kHz 190 146 - 236

More Information
Spring Constant (Nominal) 48 N/m
Spring Constant $48.00
Frequency (Nominal) 190 kHz
Frequency $190.00
Allow Set Quantities Yes
Featured Yes
Specs

Tipless, Long Tapping Mode AFM Cantilever