Ordering Information | ||
---|---|---|
Wire Length | Part Number | Price |
50 cm | 20105 | $123.50 |
100 cm | 20110 | $188.50 |
5 meters | 20115 | $864.50 |
STM tip wire is 80% Pt, 20% Ir with a 0.25 mm diameter. It is ideal for any Scanning Tunneling Microscope requiring wire of this diameter. STM tips are made by manually cutting the wire to the desired length using quality wire cutters.