Nanosensors SSS-NCH

As low as $757.00
In stock
SKU
SSS-NCH -(select options)

SuperSharp, Tapping Mode AFM Probe

Ordering Information

Quantity

Coating

Part Number

Price
10 
probes
None SSS-NCH-10
$757.00
Al reflex SSS-NCHR-10
20 
probes
None SSS-NCH-20
$1,355.00
Al reflex SSS-NCHR-20
50 
probes
None SSS-NCH-50
$2,988.00
Al reflex SSS-NCHR-50


NANOSENSORS™ SSS-NCH AFM probes are designed for non-contact mode or tapping mode AFM.

For enhanced resolution of nanostructures and microroughness we offer our SuperSharpSilicon™ tip with unrivalled sharpness.

The probe offers unique features:

  • guaranteed tip radius of curvature < 5 nm
  • typical tip radius of curvature of 2 nm
  • typical aspect ratio at 200 nm from tip apex in the order of 4:1
  • half cone angle at 200 nm from apex < 10°
  • monolithic material
  • highly doped silicon to dissipate static charge
  • chemically inert
  • high mechanical Q-factor for high sensitivity

Cantilever data:

Property Nominal Value Specified Range
Thickness /µm 4 3.0 - 5.0
Mean Width /µm 30 30 - 45
Length /µm 125 115 - 135
Force Constant /(N/m) 42 10 - 130
Resonance Frequency /kHz 330 204 - 497



More Information
Spring Constant (Nominal) 42 N/m
Spring Constant $42.00
Frequency (Nominal) 330 kHz
Frequency $330.00