QSensor QSX 309 Al2O3
QSensors are developed and produced to provide you with stable, reliable and reproducible data. Full performance is ensured through extensive quality controls and guaranteed for one-time use according to the recommendations.
Sensor Specifications | |
---|---|
Typically ships within | 3 weeks |
Part Number | QSX 309 |
Top coating material | Aluminum Oxide (Al2O3) |
Surface roughness | < 2 nm RMS |
Maximum temperature | 150 °C |
Pre-cleaning of sensor | A new sensor might be contaminated with hydrocarbons and dust. Pre-cleaning the surface will give more reproducible QCM-D results. |
Protocol | For light cleaning, step 2 – 4 below can be used.
|
Usage | QSensors are intended for one-time use only. |
Storage | Store in a cool, dry place out of light. |
Shelf life | Stable at least 12 months from package date in unopened package, see expiry date on package. |
Chemical compatibility | Do not expose to strong acids and bases. Stay within pH 4-9 to avoid corrosion. There is no guarantee that the coating will be stable under all experimental conditions. |