Description
QSensors QSX 303 Silicon Dioxide (thin)
QSensors are developed and produced to provide you with stable, reliable and reproducible data. Full performance is ensured through extensive quality controls and guaranteed for one-time use according to the recommendations.
| Sensor Specifications | |
|---|---|
| Typically ships within | < 1 week |
| Part Number | QSX 303 |
| Top coating material | Silicon dioxide (SiO2) (50 nm) |
| Surface roughness | < 1 nm RMS |
| Maximum temperature | 150 °C |
| Pre-cleaning of sensor | A new sensor might be contaminated with hydrocarbons and dust. Pre-cleaning the surface will give more reproducible QCM-D results. |
| Protocol | For light cleaning, step 1, 4 and 5 below can be used.
|
| Usage | QSensors are intended for one-time use only. |
| Storage | Store in a cool, dry place out of light. |
| Shelf life | Stable at least 18 months from package date in unopened package, see expiry date on package. |
| Chemical compatibility | Do not expose to strong bases. There is no guarantee that the coating will be stable under all experimental conditions. |